Roofing Desaturation

See Haag's exclusive and ground-breaking research at work:

 

Contact Research/Testing.

Roofing Desaturation Analysis

Bituminous Roofing samples are examined and documented, then desaturated in a vapor degreaser. We examine extracted reinforcements for fractures or strained regions characteristic of an impact. Then, we compare conditions in reinforcements with overlays of original samples. Our licensed engineer completes a report with descriptions, findings and photographs.

Request Haag Roofing Desaturation

Haag Roofing Desaturation Analysis shows fractures or strained regions in a shingle